Back     Parameters for Product description   Hot-dip galvanized barbed wire - Weight of coating 69 g/m2 (2mm)    

#Parameter CostLab
1Barbed wire formation 20,000/=Materials Lab
2Dimensions 20,000/=Materials Lab
3Length per kilogram 20,000/=Materials Lab
4Mass of zinc coating 65,000/=Chemistry Lab
5Tensile properties 70,000/=Materials Lab
Sub Total: 195,000/=